        1. excessive width  熔寬過剩

        2. insufficient width 熔寬不足

        3. excessive reinforcement 焊縫增強(qiáng)過量

        4. insufficient reinforcement 焊縫增強(qiáng)不足

        5. mismatch 錯位

        6. incomplete filled groove 坡口未填滿

        7. pit 弧坑

        8. burn through 焊穿

        9. slag inclusion (single-pass weld) 夾渣(單道焊)

        10. slag inclusion (multiple-pass weld) 夾渣(多道焊)

        11. undercut  咬邊,咬肉

        12. overlap 焊瘤

        13. porosity (along entire length of weld bead) 氣孔(沿整個焊道)

        14. wormhole porosity 蟲狀氣孔

        15. centerline crack 焊道中心縱向裂紋

        16. underbead crack 焊道下裂紋

        17. transverse crack 橫向裂紋

        18. crater crack 弧坑裂紋

        19. root crack 根部裂紋

        20. fish eye 魚眼,白點(diǎn)

        21. line inclusion 鏈狀夾雜物

        22. excessive spatter 嚴(yán)重飛濺

        23. incomplete fusion 未熔合

        24. incomplete penetration 根部未焊透

    更多翻譯詳細(xì)信息請點(diǎn)擊:http://www.trans1.cn
     
    關(guān)鍵詞: 焊接 缺陷 術(shù)語
    [ 網(wǎng)刊訂閱 ]  [ 專業(yè)英語搜索 ]  [ ]  [ 告訴好友 ]  [ 打印本文 ]  [ 關(guān)閉窗口 ] [ 返回頂部 ]
    分享:

     

     
    推薦圖文
    推薦專業(yè)英語
    點(diǎn)擊排行
     
     
    Processed in 0.207 second(s), 17 queries, Memory 0.9 M